Search results for "Hydroxyl value"
showing 2 items of 2 documents
Renewable polyol obtained by microwave-assisted alcoholysis of epoxidized soybean oil: Preparation, thermal properties and relaxation process
2019
[EN] The soybean oil polyol (SOP) use as feedstock in the polyurethane industry has been recently emphasized due to its excellent resistance to hydrolysis, which is also applicable in coatings and thermal insulation. In this article, the SOP was obtained by a very fast microwave-assisted alcoholysis of epoxidized soybean oil (ESO). The preparation method, thermal properties, and relaxation process were evaluated. High yields as opening and consumption epoxy group and selectivity of 99.8 mol%, 985 mol%, and 71.2 mol% were obtained. Through titrations, nuclear magnetic resonance and gel permeation chromatography were identified parameters as 0.32 mg KOH.g(-1) acid number, 190 mg KOH.g(-1) hyd…
Water-Blown Polyisocyanurate Foams From Vegetable Oil Polyols
2008
Polyols with the hydroxyl value OHV from 290 to 318 mg KOH/g are synthesized from rapeseed, sunflower seed, flaxseed, or coconut oils by the way of their: (1) transesterification with triethanolamine or (2) amidization with diethanolamine. The influence of water as the blowing agent on the storage stability of the polyol premix system is assessed from values of the polyol premix system pH, acid value, and variations in such parameters as cream and gel time. Water-blown polyisocyanurate (PIR) foams (150 · II × 300; II—isocyanate index) characterized by good mechanical characteristics, dimensional stability at 70°C and at relative humidity RH = 95% as well as by a very low water absorbance, …